I would appreciate information on the closest EN standards in terms of chemistry and mechanical properties to the following ASTM standards. I realize the equivalence may not be exact particularly in the mechanical certification tests.
The ASTM standards are castings and are:
A 351 grade CF8M
and A 216 grade WCB
Thanks,
The ASTM standards are castings and are:
A 351 grade CF8M
and A 216 grade WCB
Thanks,





RE: Looking for 2 EN metal casting standards
ASTM A351, grade CF8M is type 316 Stainless Steel. The chemical composition is:
0.08% C, 1.50% Mn, 2.00% Si, 9.0 to 12.0 % Ni, 18.0 to 21.0% Cr, 2.0 to 3.0% Mo.
Rao Yallapragada
Rao Yallapragada
RE: Looking for 2 EN metal casting standards
http
Rao Yallapragada