job switch
job switch
(OP)
whent from cars too to plastic terminals injection molding I just run the parts now but looking to advance bye learning to adjust the machine too stop perosity & no fill and sticking to the plate the machine is a transfer you add the plastic by cups .. trying not to look dum ... all i know this far is speed preasure and heat all work together... help






RE: job switch
Regards
eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.