Repairing cracks in concrete walls
Repairing cracks in concrete walls
(OP)
Can someone give me information about crack repairs in concrete walls (Equipment & products to be used)!!!
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Repairing cracks in concrete walls
|
RE: Repairing cracks in concrete walls
Most common method of crack repair in concrete is pressure injection of epoxy, though carbon fiber overlays and other techniques can be used depending upon the type of crack and the required performance of the repair.