I would like to know if a 3" Class 300 flange will bolt up with no problems to a 3" Class 600 flange? I work for a Process and Pipeline Company in Canada and we are going to be purging (with Nitrogen) a line for a client.
Due to such short notice all we have is a Class 300 flange and the tie in point we are using is a Class 600 (both raised face). There is no pressure on the line and will not have any other then the back pressure from us pumping Nitrogen.
Clay Culver
I would like to know if a 3" Class 300 flange will bolt up with no problems to a 3" Class 600 flange? I work for a Process and Pipeline Company in Canada and we are going to be purging (with Nitrogen) a line for a client.
Due to such short notice all we have is a Class 300 flange and the tie in point we are using is a Class 600 (both raised face). There is no pressure on the line and will not have any other then the back pressure from us pumping Nitrogen.
Clay Culver





RE: Class 300 & 600 flange Question
BigInch
-born in the trenches.
http://virtualpipeline.spaces.msn.com
RE: Class 300 & 600 flange Question
RE: Class 300 & 600 flange Question
For both B16.5 #300 & #600 shows Bolt Circle Diameters, and Hole Diameters 2b the same.