INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Stress Strain curves

Stress Strain curves

Stress Strain curves

(OP)
Does anyone know where I can find stress strain curves for aluminum alloys, particularly 6005-T5?

RE: Stress Strain curves

Mil-Handbook-5/MMPDS-01/MMPDS-02.  See various posts in the Aircraft Engineering forum for sources.

RE: Stress Strain curves

good try SW, but there isn't a 6005

RE: Stress Strain curves

(OP)
NO 6005???

MatWeb Data Sheet                
                
Aluminum 6005-T5                Date: 11/15/2006 1:15:02 PM
                
                
KeyWords:                
UNS A96005; ISO AlSiMg; Aluminium 6005-T5; AA6005-T5                
"SubCat: Aluminum Alloy, Nonferrous Metal, 6000 Series Aluminum Alloy, Metal"                
Material Notes:                
"Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN."                
                
Component    Value    Min    Max    
"Aluminum, Al"        97.5    99    
"Chromium, Cr"            0.1    
"Copper, Cu"            0.1    
"Iron, Fe"            0.35    
"Magnesium, Mg"        0.4    0.6    
"Manganese, Mn"            0.1    
            0.05    

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources