INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Temperature Derating fcator

Temperature Derating fcator

Temperature Derating fcator

(OP)
Hi

  I am trying ot find the temperature derating factor of the below materials

1. AISI 4140 (YTS 80K PSI)
2. MONEL K500 (YTS 95K PSI)
3. AISI 630 (YTS : 105K PSI)

The specified yeild strength are for ambient temperature. But i am trying to find the yeild strength at 120 degree and i believe it is going to change. Is there a formula or a data sheet or any method for determining the derated yeild strength.

Chellappan
Mechanical Engineer


RE: Temperature Derating fcator

120 deg F or 120 deg C?

RE: Temperature Derating fcator

(OP)
120 degree C

Chellappan

RE: Temperature Derating fcator

I also forgot to mention that Military Handbook, Mil-hdbk-5h, December, 1998 also has excellent information pertaining to strength reduction factors for 4140 and other alloys. You can search for a free copy of this document over the internet, as well.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.