Thermoplastic rubber to metal bonding
Thermoplastic rubber to metal bonding
(OP)
Hi, Is it possible to bond steel to thermoplastic rubber while overmoulding the steel in an injection moulding process?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Thermoplastic rubber to metal bonding
|
RE: Thermoplastic rubber to metal bonding
New mould design?
thread711-165134
RE: Thermoplastic rubber to metal bonding