INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

PSV Vent To Atmosphere

PSV Vent To Atmosphere

PSV Vent To Atmosphere

(OP)
Hi Everyone,

Some of the PSV's vents provided in Distillation Towers are routed to Atmosphere (if they  pop up), not to flare as done normally. This is the case in most of Lighter  hydrocarbons handling equipments like in Deethaniser and Ethylene tower. why  cant we put them into flare? .IS there any specific reason behind it ?

Your Opinions Plz.

thanx

RE: PSV Vent To Atmosphere

Check local environmental regulations. I believe that in the area I'm familiar with if any of the PSV's on top of the atmospheric or vacuum columns ever actually pops (I'm told that's nearly impossible) then the PSV's would have to be routed to the flare. In essence their venting to the atmosphere was grandfathered in as long as they "behave".

jt

RE: PSV Vent To Atmosphere

Money?  The flare will operate at 100 F in the day and when the PSV opens it will be -121 F. Metallurgy, expansion loops, diameter, huge diameters, segragated cryogenic (water free) flare headers, and other issues (?) .......

Ethane is not a regualated VOC, I'm not sure about ethylene. So that is not always a factor

Finally, These products will disperse and not become a fire safety issue unless the outside temperature was really cold and the don't vaporize.

RE: PSV Vent To Atmosphere

(OP)
thanx for your inputs

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources