INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Large plastic deformation of a thin plate

Large plastic deformation of a thin plate

Large plastic deformation of a thin plate

(OP)
Hi everyone,

i'm analysing a screwjoint in abaqus cae 6.5.
Its a joint with two thin plates of aluminium connected by a self-tapping screw.
To determine the shearforce-resistance of the joint the two plates are applied with a deformation of 3mm among eachother. After 1mm there are very large plastic deformations at the thinner plate an it becomes thicker so the resistance grows further. In reality the screw cuts the thinner plate and does not push the whole material in front of it. Does anyone know how to handle this problem ?

Thanks very much for any help
Greets from Europe
Nelso

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources