Does anyone of you have any idea the type of material and the exact composition of SB 111-687 material.
I looked in to the appropriate tables but with little luck,
thank you in advance,
Dimitris
Does anyone of you have any idea the type of material and the exact composition of SB 111-687 material.
I looked in to the appropriate tables but with little luck,
thank you in advance,
Dimitris





RE: SB 111-687 ???
The metal is Alumininum Brass, B
UNS Designation C68700
Contents
Copper 76.0-79.0
Aluminum 1.8-2.5
Lead 0.07 Max
Iron 0.06 Max
Arsenic 0.02-0.10
Zinc Remainder