Grinding PTFE Coated 304 SS
Grinding PTFE Coated 304 SS
(OP)
We flate grind the ends of PTFE coated SS wire that has been coiled into a heliz. We always have problems with strings of the PTFE hanging from the ground end. Has anyone had a simlar problem they have solved?