INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

A Numbers, Qw 442

A Numbers, Qw 442

A Numbers, Qw 442

(OP)
Can anyone tell me what (A) number does ENiCrMo-4 have, and why does Section II part (c) not reference it.

RE: A Numbers, Qw 442

There is no A-No because the A-No Classifications are for ferrous material per ASME Section IX, QW-442. The F-No for this Ni-base filler metal is F-No 43.

RE: A Numbers, Qw 442

(OP)
Thanks Metenger,
                 Since the Classification for these electrodes has a Low Carbon and (Fe) content specified, I assumed it would have an (A) number..
I thought all non ferrous metals had no (Fe) content..
Thanks...

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources