S-N curve for P265GH?
S-N curve for P265GH?
(OP)
Hi,
I am looking for the S-N curve of P265GH (EN 10 028-2) pressure vessel steel. The designation for this material in
- DIN is HII
- ASTM/ASME is A 516 GR 60.
I need the curves in order to carry out a pressure vessel fatigue analysis where the mentioned material is used.
Alternatively, I will be exteremly grateful if some one could provide me with the following information about this material :
1- Strength coefficient (sigma f)
2- strength exponent (b)
3- Ductility coefficient (epsilon f)
4- Ductility exponent (c)
Once again thank you for you help!
I am looking for the S-N curve of P265GH (EN 10 028-2) pressure vessel steel. The designation for this material in
- DIN is HII
- ASTM/ASME is A 516 GR 60.
I need the curves in order to carry out a pressure vessel fatigue analysis where the mentioned material is used.
Alternatively, I will be exteremly grateful if some one could provide me with the following information about this material :
1- Strength coefficient (sigma f)
2- strength exponent (b)
3- Ductility coefficient (epsilon f)
4- Ductility exponent (c)
Once again thank you for you help!