INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

What is st6wf13.5? What is the flange/web size?

What is st6wf13.5? What is the flange/web size?

What is st6wf13.5? What is the flange/web size?

(OP)
I have a drawing that calls for:
st6wf13.5x7'-2 1/2"

and
st15wf54x25'-11"

From the machinery's hand book, I am pretty sure it is  structural "T" and it is, 6 and 15 inches in height and 13.5 and 54 lbs per ft.

My problem is I have searched the hand books that I have and the internet but I can't find the dimensions of the flange and web.

The building was erected in the 60s in Canada. Some of the steel is from Scotland.

Any help would be appreciated.
Erik

RE: What is st6wf13.5? What is the flange/web size?

I think you got it.  It is almost certainly a structural T cut from a W shape with the given height and weight per foot.  I guess you just need to get a European steel shape table from the appropriate era.  Maybe someone at AISC may be able to help.

I presume the shapes are near the ones given for a WT6x13 and WT15x54 in todays AISC manual.  Good Luck

RE: What is st6wf13.5? What is the flange/web size?

This is likely a structural tee cut from a W12X27 beam... and is 7'-2-1/2" long.  The W12X27 has a 6-1/2" flange width.

Dik

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources