INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Is the allowable stress of SA-516 70N same as SA-516 70?

Is the allowable stress of SA-516 70N same as SA-516 70?

Is the allowable stress of SA-516 70N same as SA-516 70?

(OP)
Dear everyone,

I could not find the allowable stress in ASME Sec II Part D for SA-516 70N. Does that mean that their stresses are the same?

Thank you.

RE: Is the allowable stress of SA-516 70N same as SA-516 70?

Yes. Grade 70 steel under ASME SA-516 must meet the minimum mechanical property requirements, hot rolled or normalized.

See thread330-75119

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources