INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASME SEC I

ASME SEC I

ASME SEC I

(OP)
hi,
Is ASME sec I allow patching at bigger hole to make it smaller as per diameter of down comer od?I.e We made offset hole on drum and now we have to move down comer appx. 1", so can we patch that 1" offset howl with the same matl. and thkness of pipe?
Also can we do PWHT again on the area where PWHT already done?
I need guidence ASAP.pls..
Thanks in advance
Mihir5577

RE: ASME SEC I


Quote:

Is ASME sec I allow patching at bigger hole to make it smaller as per diameter of down comer od?I.e We made offset hole on drum and now we have to move down comer appx. 1", so can we patch that 1" offset howl with the same matl. and thkness of pipe?
Also can we do PWHT again on the area where PWHT already done?

Reply; Yes, if approved by the AI.

RE: ASME SEC I

I agree with metengr.

I would ask you to submit a suitable repair procedure that is supported by your QC System.

RE: ASME SEC I

how big a hole?
you may not even need to PWHT again, check for pWHT requirements and your AI,
genb

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources