ASTM A262 rapid screening test
ASTM A262 rapid screening test
(OP)
The rapid screening test suggests an applied voltage of 20V. If the current density is achieved for the sample size does the voltage applied have any significant effect? or will any reasonable voltage less than 20V still achieve an acceptable result?
Any suggestions or thoughts would be appreciated.
Any suggestions or thoughts would be appreciated.