ASTM B-117 Salt Fog Testing....where?
ASTM B-117 Salt Fog Testing....where?
(OP)
Can anyone recommend, worldwide, a good facility to do this test for a small company on a tight budget?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
ASTM B-117 Salt Fog Testing....where?
|
RE: ASTM B-117 Salt Fog Testing....where?
http://mt.bodycote.com/
You may want to ask for ISO 9227, which is essentially the same as ASTM B 117.
Regards,
Cory
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
RE: ASTM B-117 Salt Fog Testing....where?
http://ww
TTFN
RE: ASTM B-117 Salt Fog Testing....where?
ck1999
RE: ASTM B-117 Salt Fog Testing....where?
Test spec: BS 3900-F12 which is identical to ISO 7253 and virtually identical to ASTM B 117. This uses a 5% aqueous solution of sodium chloride. The cabinet is operated at 35°C.
http:/
RE: ASTM B-117 Salt Fog Testing....where?
Actually what we are struggling to find (at a good price) is the ASTM G53 (or superseeded version) UV B testing, this seems a bit rarer.
Oh, PS - It has to be B117 - I'm not a fan of the test but that's the spec' we have to match unfortunately, there are much better 'realistic' tests around I know (grumble)...
RE: ASTM B-117 Salt Fog Testing....where?
http://www.atlas-mts.com/
Regards,
Cory
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.