INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

"0" Condition

"0" Condition

"0" Condition

(OP)
This may be a simple question but I'm not at all fimilar with welding. What is the "0" condition.

Thanks for the help.

RE: "0" Condition

With respect to what material?

RE: "0" Condition

Take Alloy Aluminum for Example

6061-0 is Annealed 6061 Alloy Aluminum

Wes C.
------------------------------
No trees were killed in the sending of this message, but a large number of electrons were terribly inconvenienced.

RE: "0" Condition

(OP)
Steel, A36 and HT 50. Thanks again.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources