RE: HCl 35% DRUM VENT SCRUBBER
dC/dt ∝ kHC
The Henry's Law constant is unfortunately not constant (should be an expression somewhere), but data for the HCl vapor pressure vs. concentration & temperature is given many places, e.g., Table 1 & Fig 1 here:
http://arc