SA-516 plate
SA-516 plate
(OP)
Is it permissable to bend SA-516 gr 70 plate for ASME code use with no further treatment? If not, where in the code could I locate that?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: SA-516 plate
For plate used in unfired pressure vessels, please review ASME B&PV Code, Section VIII, Div 1, Part UCS-79.
For plate used in ASME Section I, boilers, there is no limitation.