Fibre Reinforced Cement Pipes
Fibre Reinforced Cement Pipes
(OP)
Has anybody come across durability problems with Fibre Reinforced Cement pipes (otherwise known as 'fibre cement') installed for up to 30 years? The fibres were originally asbestos, now cellulose.
I am beginning to investigate some failures of these pipes when installed 'architecturally' as a cantilever and suspect they can deteriorate from rainwater (soft water attack perhaps?).
I am beginning to investigate some failures of these pipes when installed 'architecturally' as a cantilever and suspect they can deteriorate from rainwater (soft water attack perhaps?).





RE: Fibre Reinforced Cement Pipes