INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

DPI crack-like indications

DPI crack-like indications

DPI crack-like indications

(OP)
Hi everybody,
I got a lab report about some cracks found on AISI 304 flanges after welding.
One of the paragraph concerns 'DPI crack-like indications', does anyboduy know what DPI means?

Thanks

RE: DPI crack-like indications

Probably dye penetrant inspection (DPI). Dye Penetrant inspection is a nondestructive testing method.

RE: DPI crack-like indications

Of course, now someone needs to confirm is they really are cracks or just surface indications.
If someone wants to grind on these make sure that they really grind them out and not just smear the metal over to cover the indications.
Is there another NDT method allowed?  Is the shape one that you could X-ray?

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
http://www.trent-tube.com/contact/Tech_Assist.cfm

RE: DPI crack-like indications

Really beats me to know that crack can occur on a50% elongation and 35% Reduction in area material. Are they by any chance cold flow marks.

RE: DPI crack-like indications

arunmrao;
My guess is weld defect(s) related to solidification type cracks.

RE: DPI crack-like indications

Yes quite right. I missed  reading the thread properly. Sorry!!I assumed it as a forged blank and then machined.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources