Welding issue
Welding issue
(OP)
A 5/16 in fillet normally does not need two passes. Correct? Is there a table indicating when more than one pass is needed? Sorry, I' am little fuzy on this. Thanks for your help.
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Welding issue