RECOMMENDATION FOR S S PIPELINE PROTECTION
RECOMMENDATION FOR S S PIPELINE PROTECTION
(OP)
Gentlemen,
We require to lay underground pipeline ( Stainless steel SA 358 TP304 L grade,12"NB Welded,10s thk,100 Metre length)at a depth of 1 to 1.5 Metre.The soil condition is little saline & the area is marine.Could you give your suggestions/recommendations for the suitable coating method such as 3 LPE or any cold coating tape for the external protection of pipeline.
Expecting your co-operation & immediate response.
Regards,
Dilip
We require to lay underground pipeline ( Stainless steel SA 358 TP304 L grade,12"NB Welded,10s thk,100 Metre length)at a depth of 1 to 1.5 Metre.The soil condition is little saline & the area is marine.Could you give your suggestions/recommendations for the suitable coating method such as 3 LPE or any cold coating tape for the external protection of pipeline.
Expecting your co-operation & immediate response.
Regards,
Dilip





RE: RECOMMENDATION FOR S S PIPELINE PROTECTION
Is double containment an option?
= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
http://www.trent-tube.com/contact/Tech_Assist.cfm
RE: RECOMMENDATION FOR S S PIPELINE PROTECTION
Agree with Ed that buried SS should be a last resort.