INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASTM equivlant for BS3602 HSF 27

ASTM equivlant for BS3602 HSF 27

ASTM equivlant for BS3602 HSF 27

(OP)

Hi guys,

if anyone has a good reference book that could tell me the ASTM equivlant for BS 3602 HSF 27 I'd be terrible grateful,

Thanks
Tony.

RE: ASTM equivlant for BS3602 HSF 27

From a cross-listing at http://www.venusent.com/td/p11.pdf#search=%22%22BS%203602%22%20%22HFS%2027%22%20ASTM%22
the equivalent is ASTM A106 Grade B.
It has a lower limit on sulfur (max 0.035 wt%) than does the 0.05% of BS 3602 HSF 27.

ASTM A106/A106M-06 Standard Specification for Seamless Carbon Steel Pipe for High-Temperature Service
http://www.astm.org/cgi-bin/SoftCart.exe/DATABASE.CART/REDLINE_PAGES/A106A106M.htm?L+mystore+cnmc6063

RE: ASTM equivlant for BS3602 HSF 27

(OP)
thanks

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources