En equivalent AISI standard material datas
En equivalent AISI standard material datas
(OP)
Hi,
I am looking for En8 equivalent materials from AISI standard.How to get these details through internet resources
Thanks in before
John
I am looking for En8 equivalent materials from AISI standard.How to get these details through internet resources
Thanks in before
John





RE: En equivalent AISI standard material datas
Search for EN8, and find AISI 1040 Steel, available with various heat & mechnical treatment. One specific example:
"AISI 1040 Steel, oil quenched from 855°C (1570°F), 595°C (1100°F) temper, 100 mm (4 in.) round
...
Key Words: UNS G10400, ASTM A29, ASTM A108, ASTM A510, ASTM A519, ASTM A546, ASTM A576, ASTM A682, MIL SPEC MIL-S-11310 (CS1040), SAE J403, SAE J412, SAE J414, DIN 1.1186, JIS S 40 C, BS 970 060A40, BS 970 080A40, BS 970 080M40 (EN8), BS 2 S 93"
Composition & properties are given, & sometimes supplier links.
RE: En equivalent AISI standard material datas
RE: En equivalent AISI standard material datas