INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Requirement for PWHT of API 661

Requirement for PWHT of API 661

Requirement for PWHT of API 661

(OP)
Hi. All,

API Standard661/ISO 13706:2001 say that as below;
9.2 Postweld heat treatment
9.2.1 All carbon steel and low-alloy steel headers shall be subjected to postweld heat treatment. Welded tube-to-tubesheet joints shall be excluded from postweld heat treatment.


Above mean is that any welding is prohibited after PWHT even repair welding for undercut. Is it correct? ( The product also required ASME Set.VIII)

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources