INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Atmospheric CSCC Threshold Temp For 6Mo

Atmospheric CSCC Threshold Temp For 6Mo

Atmospheric CSCC Threshold Temp For 6Mo

(OP)
We are probably all aware of the universally adopted limit of 60 deg C as the threshold temperature for CSCC of 316/316L stainless steels; however, the limits for 6Mo austenitics are not so readily discernible.  Does anyone using these materials have a specified threshold temperature for CSCC under atmospheric exposure (marine, industrial, whatever)?

Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdo/

RE: Atmospheric CSCC Threshold Temp For 6Mo

I have never seen CSCC in AL-6XN in the lab below 122C.  I have never seen CSCC in a real application below 155C.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
http://www.trent-tube.com/contact/Tech_Assist.cfm

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources