INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Press Fit (thin wall SS tube)

Press Fit (thin wall SS tube)

Press Fit (thin wall SS tube)

(OP)
Hi

Need some help in designing a press - interference fit

We have a 6-4 Titanium collar (OD 22.2mm ID TO BE DETERMINED) which we currently connect by loctite to a:

14.1mm OD,
13.1mm ID
304 Stainless tube (not annealed)
6mm insertion of tube into the titanium

Despite our best efforts the loctite works 95% of the time only!

I wonder if someone could help us design the ID of aperture in the titanium part- for a press fit

The press force available would be that normally availble in workshops only

We out source production and want to make some best guess prototypes, and as you know titanium is expensive +

Cheers Simon

RE: Press Fit (thin wall SS tube)

Hi notTiger

Please don't double post I have answered your question in
thread404-151892


regards desertfox

RE: Press Fit (thin wall SS tube)

(OP)
Sorry about the double post _ I didn't see it as I hadn't realised I was posting to an existing topic

Cheers

Simon

RE: Press Fit (thin wall SS tube)

Loctite won't work reliably if there is a press fit. Read the application notes for whichever Loctite product you are using.

Seee the FAQ section for a calculator for press fits.

Cheers

Greg Locock

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips.

RE: Press Fit (thin wall SS tube)

(OP)
Thanks Greg - that is a great resource - Isn't the webwunnerful!

Cheers Simon

www.pukugolf.com

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources