INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Anodized aluminum on International Space Station

Anodized aluminum on International Space Station

Anodized aluminum on International Space Station

(OP)
I noticed an article on the ISS on the Aluminum Extruders Council website.  Not really new, but it specifically mentions why the aluminum was anodized:

"...The anodized surface finish on the extrusions provides superior optical properties, because anodized aluminum doesn’t get as hot, giving better overall thermal control.”

"Handrails are anodized in a bright gold * finish to stand out visually against the clear silver truss structures—an essential point of safety for every crewmember on an EVA."

http://www.aec.org/assets/pdfs/ShowcaseSeptMag9low.pdf
*Pretty certain this is an inorganic dye based on Fe, commonly known as Gold 4N.

RE: Anodized aluminum on International Space Station

Anodizing is also done to prevent cold/vacuum welding if two like metal objects come into contact.

BTW- First post here to this here great forum!  :)

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources