INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

MDMT for Alky reactors and contactors

MDMT for Alky reactors and contactors

MDMT for Alky reactors and contactors

(OP)
Are there any special rules for determining the MDMT for alky reactors/contactors or can I just apply the rules of ASME VIII UCS-66?

RE: MDMT for Alky reactors and contactors

hello,

the minimum operating temperature will be reached if the pressure vessel is opened to the atmosphere, on this calculated temperature a design margin should be added.

regards,
         roker
 

RE: MDMT for Alky reactors and contactors

This is really more of a question for forum794 but as far as I know, VIII-1 does not require anything beyond UCS-66.

jt

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources