Corrosion Rate
Corrosion Rate
(OP)
Is there any reference material or charts for predicting the rate of corrosion for various steel including zinc plated steel under different environments (moisture, de-icing salt, salt air from the sea…)?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Corrosion Rate
Suggest 'Corrosion of Carbon and Alloy Steels,' pp. 5-53 in ASM Handbook, Volume 13B, Corrosion: Materials, (2005), especially 'Corrosion of Metallic Coated Steels,' pp. pp. 35-39. http://w
Or, see pp. 509-582 in the previous edition, ASM Handbook, Volume 13, Corrosion (1982).
ASTM B633, "Standard Specification for Electrodeposited Coatings of Zinc on Iron and Steel," gives some average corrosion rates for zinc coatings in different atmospheres.
For industrial atmospheres: 5.6 microns/year,
For Urban non-industrial or marine atmospheres: 1.5 micron/year.*
http:/
*but the conditions you've described here & in thread332-156141 and thread332-160274 are more severe than the average marine atmosphere of ASTM B633.