Factors influencing weld toe to toe distance requirements
Factors influencing weld toe to toe distance requirements
(OP)
We would like to cut out a 16mm butt weld on an existing precipitation tank, and place a new weld only approximately 100mm from where the old weld was. This is far less than that specified in API 650. We can test a sample of the weld and plate around the HAZ; do we need to look for metallography changes only, or are there other factors that influence weld toe to toe distances?





RE: Factors influencing weld toe to toe distance requirements
What standard was the tank fabricated?
RE: Factors influencing weld toe to toe distance requirements
RE: Factors influencing weld toe to toe distance requirements
forum809