INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Fire Retardant and Pressure Treated Wood

Fire Retardant and Pressure Treated Wood

Fire Retardant and Pressure Treated Wood

(OP)
Is fire retardant wood available that is also pressure treated or have some other form of decay or moisture resistance? Does fire treated wood alone have some resistance to decay?

RE: Fire Retardant and Pressure Treated Wood

Yes, but with restrictions. Wood treated with borate compounds is decay Resistance, fire resistant, and available ...but not moisture resistant. Here is a typical product
http://www.durable-wood.com/pdfs/borate-eng1oct02.pdf

The Forest Products Lab has looked into this situation, but I don't believe the combinations of treatments discussed here are readily available
http://www.fpl.fs.fed.us/documnts/fplrp/fplrp545.pdf

www.SlideRuleEra.net idea

RE: Fire Retardant and Pressure Treated Wood

Check with some one who does fire retardent pressure treating.  It was my understanding in the past that Dricon had some decay resistance.

 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources