INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

JIS TO EN CONVERSION FOR FABRICS

JIS TO EN CONVERSION FOR FABRICS

JIS TO EN CONVERSION FOR FABRICS

(OP)
I need help for the following questions:
- test result on water vapour permeability for clothes, done according to JIS L1099 Method B-1:1993 (the result is 15156 grams for square meter for 24 hours) can be somehow compared with UNI 48418 or EN343/03 standard for water permeability (expresses in the same units)?
- test result on hydrostatic pressure on the same fabric, done according to JIS L1092-1998 section 6.1.2 method B (the result is 10.000 mm) can be compared to EN 20811/93 or EN343/03 standard (expressed in the same units)?
I'd lik to know the conversion coefficient (if exists).
Thanks to anyone who will help
luca

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources