I have a weldment - mild steel square tubing - that I wish to give an oxidized or "premature" rusted finish to, strictly for aesthetic purposes. Its for an outdoor ornamental product.
Can anyone help me with a process - chemical application or like - to achieve this finish?
Thanks!
Can anyone help me with a process - chemical application or like - to achieve this finish?
Thanks!





RE: Oxidized Finish
RE: Oxidized Finish
RE: Oxidized Finish
http://www.welding-advisers.com/
RE: Oxidized Finish
If you have finished it one way to accelerate rusting is to expose the surface to a salt spray. The structure will have to be cleaned by blasting so you will have a more uniform rusting.
RE: Oxidized Finish
You know that these will continue to rust and they will bleed where there is runoff?
= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
http://www.trent-tube.com/contact/Tech_Assist.cfm