Smart questions
Smart answers
Smart people
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Member Login

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips now!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

Join Eng-Tips
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

LINK TO THIS FORUM!

Add Stickiness To Your Site By Linking To This Professionally Managed Technical Forum.
Just copy and paste the
code below into your site.

Partner With Us!

"Best Of Breed" Forums Add Stickiness To Your Site
Partner Button
(Download This Button Today!)

Feedback

"...Since using forums in my early days 10 years ago in CompuServe, one had to log back on and sometimes wait days for a response. Now I get a response e-mailed to me which I can click a link and go right back to exactly where My post was..."

Geography

Where in the world do Eng-Tips members come from?
Bergg (Mechanical)
5 Jul 06 16:10
Have been asked by a customer to mold a 3/4 inch thick  9 inch dia flexible disk with a hole in the center.

Understand that it fits on the arm to help swimmers float.

Would like some idea of what materials would be best to make this happen.

Thanks

Bergg
patprimmer (Publican)
5 Jul 06 19:51
Closed cell EVA foam, as used for the soles of rubber thongs and for "Boogy Boards"

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.

Bergg (Mechanical)
6 Jul 06 12:48
patprimmer:

Thanks I will follow this up.  I assume that EVA can be injection molded.

Regards:

Bergg
dwightdixon (Materials)
11 Jul 06 8:04
I presume they want to foam the part. If you want a more flexible material than EVA I suggest you look into foamed TPE.  Many of these arm bands are made from foamed Kraton based material. You can buy from GLS in the US 800-457-8777.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!

Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close