Inconel tubing compatibility
Inconel tubing compatibility
(OP)
Does anyone have any info they could give me on the compatibility of inconel tubing and a phosphoric acid compund? I am using hasteloy tubing at the moment, however I am need to add an additional injection point to my production stream and am looking to save on costs.





RE: Inconel tubing compatibility