INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Appendix L Fig.L-1.4-1

Appendix L Fig.L-1.4-1

Appendix L Fig.L-1.4-1

(OP)
In Fig.L-1.4-1 in Appendix L of ASME Sect.VIII Div.1, 2005 Addenda. If my cylinder is seamless section, I will select RT of Category B and C butt joint, and the figure will shown joint efficiency of category A B and C.But cylinder is seamless section, why category A have Type 1 or Type 2.(In UW-12 (d): seamless section shall be considered equivalent to welded parts of the same goemetry in which all Category A welds are Type No.1)

RE: Appendix L Fig.L-1.4-1

I do not get the q,
it may be the weld full or welds w/backing in the latest it will make it lower,
genb

RE: Appendix L Fig.L-1.4-1

In order to obtain the E = 1.0 on seamless vessel sections, one must perform spot RT of the B seam that join them.  Otherwise E = 0.85 for a seamless section w/o spot RT.  See the dreaded UW-11a)5b).

Steve Braune
Tank Industry Consultants
www.tankindustry.com

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources