INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Performance of Super Duplex Stainless Steels

Performance of Super Duplex Stainless Steels

Performance of Super Duplex Stainless Steels

(OP)
Does anyone have any experience with the performnace of superduplex stainless steels (UNS S32760 or S32750) in caustic solutions (10% NaOH wt) with 1% - 5% sulfides wt. at temperatues around 250 F?  Thanks.

RE: Performance of Super Duplex Stainless Steels

No, I don't have any specific info.
However these alloys do very well in dilute caustic environments.  The NaS does not have much impact on corrosion at these lower concentrations.
How are you getting to 250F?  Boiling should be about 220F.

Check out the Outokumpu corrosion info on line.
http://www.outokumpu.com/applications/documents/start.asp

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
http://www.trent-tube.com/contact/Tech_Assist.cfm

RE: Performance of Super Duplex Stainless Steels

(OP)
The temperature of 250 F is due to 15 psig pressure.  

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources