INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Costs / Bogey Numbers

Costs / Bogey Numbers

Costs / Bogey Numbers

(OP)
We have a plethora of small steel weldments, ie:
knee braces, usually 3x 3x 3/8  x  4 foot overhang
Short pipe stands with end 1/4" plates, 4'WF usually 4 ft high
6 ft sq low level platform step-ups about 21" high

All are C.S. and primed / gray spray epoxy

Need is to rough cost for domestic fabrication based on poundage

What would be the current cost per pound out of a local fab shop?

Same question if all were hot dipped galvanized?

RE: Costs / Bogey Numbers

Shopper,

I have bought steel here in the U.S. in the past year for the following prices:

GALVENIZED C.S.:
700lb @ 2.11$/lb
725lb @ 2.2$/lb
13500lb @ 1.5$/lb
44500lb @ 1.34$/lb

Non-Galvenized C.S.:
590lb @ 1.61$/lb

I notice you post was a few weeks ago so you may have already purchased, if so, I would like to hear your prices...

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources