ASTM Equivalency for 1144 Straight
ASTM Equivalency for 1144 Straight
(OP)
Can anyone tell me if there is an ASTM standard that is equivalent to AISI 1144 Straight (not Stressproof and not stress-relieved).
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
ASTM Equivalency for 1144 Straight
|
RE: ASTM Equivalency for 1144 Straight
SAE J403 - Chemical composition only
SAE J935 - High strength die-drawn bar standard, with 1144 being one of the grades
ASTM A 29 - Hot rolled bar standard, with 1144 being one of the grades
ASTM A 108 - Cold drawn bar standard, with 1144 being one of the grades
The choice of ASTM standard depends on the product form (cold-drawn bar, hot-rolled wire rod, etc.) that is required.