Machining Ceramic
Machining Ceramic
(OP)
I'm making a heat barrier for a machine out of the ceramic Macor.What is the easiest way to machine this e.g. cutters,speeds and feeds ?Thankyou.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Machining Ceramic
http://
RE: Machining Ceramic
ht
http://www.azom.com/details.asp?ArticleID=1440
http://www.astromet.com/macor.htm
Regards,
http://www.welding-advisers.com/