INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Corrosion of 487-2C on production platform

Corrosion of 487-2C on production platform

Corrosion of 487-2C on production platform

(OP)
I'm looking for reasons why a 487-2C material would corrode with only slightly lower Ni,Cr,Cu content than an adjacent item.  Both meet ASTM requirements for proper classification.  487-2C has no lower bounds for these alloying elements.  An item with .09Cr,.09Ni,.16Cu Wt% corroded within one week in a sweet crude environment, prior 487 item had a 20 year history.  A mill coating or machine fluid has been speculated, but no evidence.    

RE: Corrosion of 487-2C on production platform

If the difference in behavior cannot be speculated, would it not be worth to launch a complete metallurgical investigation?

http://www.welding-advisers.com/

RE: Corrosion of 487-2C on production platform

Small diferences in Cr may have an impact, but my money is on either microstructure (thermomechanical history) or surface condition.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
http://www.trent-tube.com/contact/Tech_Assist.cfm

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources