INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Regarding NACE

Regarding NACE

Regarding NACE

(OP)
Recently I am interested in NACE, lots of petroleum and natural gas pipeline valve need manufactured in terms of it. I am wondering how a company identify its capacity to implement NACE, or it could be provided authorized certificate by this organization similar as API6D monogram.

 Thanks!

RE: Regarding NACE

NACE approves/certifies materials for sour service (as I understand it).  

Thus, when you specific NACE materials for valves, piping, etc, the vendor has to provide acceptable materials along with the supporting documentation.  NACE also gets into other requirements such as maximum hardness for welds but I have only a very general understanding of it.

RE: Regarding NACE

You will not get a manufacturing facility certified to NACE.  What would be a useful start though, is to have the facility certificated to ISO 9001/ISO 29001.  NACE themselves also do NOT certify materials; that is down to the supplier in accordance with ISO 10474 or EN 10204, for example.

Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdo/

RE: Regarding NACE

(OP)
Thank you TD2K and  SJones!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources