INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Values of Coefficient Y for Inconel 600 & 625

Values of Coefficient Y for Inconel 600 & 625

Values of Coefficient Y for Inconel 600 & 625

(OP)
HI All,

To calculate thickness of the pipe. I am looking for the values of coeffiicent (Y)for Inconel 600 and Inconel 625. ASME B313.3 list the Y vaues for Ferritic steels and some others but not for nickel alloys.

Can anyone help me out.

Thanks in advance.    

Asif Raza

RE: Values of Coefficient Y for Inconel 600 & 625

did you try google?

regards,
         roker

RE: Values of Coefficient Y for Inconel 600 & 625

Table 304.1.1 specifies 0.4 for "other ductile materials" so that is what you have to use.

RE: Values of Coefficient Y for Inconel 600 & 625

(OP)
Thanks a lot guys for your help.

Asif

Asif Raza

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources