III NH has properties for 2 1/4Cr-1Mo. I would like to know the UNS number of this alloy? Where can I find the UNS for the alloys listed in NH?
Thanks.
Thanks.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Section III NH question
Castings UNS J21890, J22091 see Section II, Part D