heat treatment
heat treatment
(OP)
is any one have some experiance about heat treatment of steel base adamite rolls i will be pleased
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: heat treatment
CODE
http://www.hitachimetals.com/product/rolls/cast/documents/AdamiteSteelRolls.pdf
http://www.brchina.com/downloads/english/steel_qualities.pdf
==========================================