Plastic Coated Dowels
Plastic Coated Dowels
(OP)
Is there an ASTM reference for plastic coated dowels as typically used in highway construction?
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Plastic Coated Dowels
RE: Plastic Coated Dowels
There are many different testing requirements. I just googled "AASHTO epoxy coated rebar specification" and AASHTO M284 came up several times. The CRSI website gave this information on this spec.
AASHTO M 284M/M 284-05
Epoxy-Coated Reinforcing Bars: Materials and Coating Requirements
Covers materials specifications and test methods commonly used in the construction of highway facilities.
Hope this helps
RE: Plastic Coated Dowels
RE: Plastic Coated Dowels
The plastic coated dowel bars are for highway slabs (shear transfer) and are set in wire baskets. They are usually yellow in color.
RE: Plastic Coated Dowels
RE: Plastic Coated Dowels
Hg